Discussion:
pad-weld practice - getting hand back after 2yrs
(too old to reply)
Richard Smith
2024-06-23 19:56:37 UTC
Permalink
Hi there

For what it's worth - other volunteer paired with not here today, so
continued to run-off pad-welds "getting hand back in".
Amazed coming back to it.
Running nicely enough.
Then used chalk and straight-edge to give me line to weld to.
That increased the number of variables being controlled...
Going to have to get out good commercial-grade autodarkening visor,
and fixed shade have "cheater" lens ("reading glasses strength"). So
can see weld more clearly than with cheaper autodarkener I restarted
with.

Good to be back though.
Going to insist the "cage" would in reality take the force if it
really were suspended from the master-link of the 4-chain bridle-set
arrangement, even though in reality with sit on a beam (the shaft is
flooded from a few metres down - was pumped "for free" by neighbouring
mine when they were naughty going beyond their sett and broke into
this mine - firmly told by judge that brought this on themselves -
pumped until that mine closed).
Make sure that if some circumstance did change, thing (the cage) will
do what it looks like it should do.

Overall - happy days...

Best wishes,
Rich S.
Jim Wilkins
2024-06-23 23:38:27 UTC
Permalink
"Richard Smith" wrote in message news:***@void.com...

Hi there

For what it's worth - other volunteer paired with not here today, so
continued to run-off pad-welds "getting hand back in".
Amazed coming back to it.
Running nicely enough.
Then used chalk and straight-edge to give me line to weld to.
That increased the number of variables being controlled...
Going to have to get out good commercial-grade autodarkening visor,
and fixed shade have "cheater" lens ("reading glasses strength"). So
can see weld more clearly than with cheaper autodarkener I restarted
with.

Good to be back though.
Going to insist the "cage" would in reality take the force if it
really were suspended from the master-link of the 4-chain bridle-set
arrangement, even though in reality with sit on a beam (the shaft is
flooded from a few metres down - was pumped "for free" by neighbouring
mine when they were naughty going beyond their sett and broke into
this mine - firmly told by judge that brought this on themselves -
pumped until that mine closed).
Make sure that if some circumstance did change, thing (the cage) will
do what it looks like it should do.

Overall - happy days...

Best wishes,
Rich S.
--------------------------------------------
The chain I buy here is sized metric though sold as the nearest inch. This
gives the working load in pounds, the ultimate strength is 4x except 3x for
G43.
https://www.myteeproducts.com/blog/chain-grades-chart/